Grade A vs Grade B steel plate
Both are 235 MPa normal-strength hull structural grades with identical tensile range and elongation — the difference is impact testing: Grade A is not impact-tested at normal thickness, Grade B is tested at 0°C.
Spec comparison
| Property | A | B |
|---|---|---|
| Giới hạn chảy tối thiểu ReH | 235 MPa | 235 MPa |
| Độ bền kéo Rm | 400–520 MPa | 400–520 MPa |
| Độ giãn dài A5 | 22% | 22% |
| Nhiệt độ thử va đập | Không yêu cầu | 0 °C |
| Tình trạng hàng | Có sẵn trong kho | Hàng trọng điểm |
How to choose
Grade B is the mill's core stock item and the more heavily stocked of the two, held in thicknesses up to 22 mm against Grade A's 12 mm ceiling — for most general hull applications B is the default. Grade A remains the right choice where the structural drawing specifically does not require impact toughness and a thinner section is sufficient. Confirm which the drawing specifies before ordering, since the two are not interchangeable once a classification society has approved a design against one of them.
Tell us the grade, thickness and tonnage.
Send grade, thickness, dimensions and tonnage. You get availability, price and a lead time, normally within 24 hours.