Engineering tool
Welding procedure qualification planner
Describe the butt weld test you plan to make. The planner shows the thickness range and steels the approval will cover, the limits that apply in production, the tests and impact notch positions the test plate needs, and the values the results must reach, from the CCS Rules for welding procedure approval.
Test conditions
Additional conditions (optional)
Approved range and production limits
Steels the procedure covers
Hover over a grade to see why.| Ordinary | A | B | D | E |
| Grade 32 | AH32 | DH32 | EH32 | FH32 |
| Grade 36 | AH36 | DH36 | EH36 | FH36 |
| Grade 40 | AH40 | DH40 | EH40 | FH40 |
Covered Confirm with the society Not covered
Tests on the test plate (3.2.4.1)
a weld centre, b fusion line, c heat affected zone 2 mm from the fusion line, d 5 mm, e 10 mm. Position d is added only when the approval will be used for important offshore structure joints (note 2).
What the results must show (3.2.5)
Interpretations and production conditions (9)
- A multi-pass procedure cannot be used for single-pass welds (3.1.4.2).
- A procedure approved on normalised, as rolled or controlled rolled steel generally covers TMCP steel too, but not the other way round (3.1.4.3 (5)).
- Each condition above stands on its own. A change beyond the covered range in any one of them generally needs a new approval test (3.1.4.1).
- Preheat temperature not lower than in the test, and interpass temperature not higher than in the test (3.1.4.11).
- If the test used post weld heat treatment or ageing, production needs it too (3.1.4.12).
- A change of current type (direct, alternating, pulsed) or of polarity normally needs a new approval (3.1.4.10).
- Consumables: the same grade as in the test, suffix included. For processes above 50 kJ/cm the rule gives no coverage statement (3.1.4.7).
- Shielding gas: a change of composition or mixing ratio is allowed only within the groups of Table 2.5.1.3 or 2.9.2.4 (3.1.4.7).
- An approval made with workshop primer covers welding without primer, but not the other way round (3.1.4.14).
What this planner covers
CCS Rules for Materials and Welding 2021, Part 3 Chapter 3: the approved thickness range (Table 3.1.4.5a), the steels a test covers (3.1.4.3), the joint types, pipe diameter, heat input, throat thickness and welding positions the approval covers (3.1.4.5 to 3.1.4.14), the test specimens and impact notch positions (3.2.4.1), and the acceptance requirements (3.2.5): tensile, bend, impact temperature and energy, hardness and macro examination. It covers hull steels A, B, D, E and the AH, DH, EH and FH grades of 32, 36 and 40.
What it does not cover
Fillet weld procedure tests, welder qualification, aluminium and stainless steel, and test joints between two different steels (the rules take the impact specimens from the lower toughness side). The conditions in production are listed only and are not checked against your procedure. The tool does not replace the approval, which is witnessed by your surveyor.
Source
Every table cell and clause above was read from the page images of the CCS Rules for Materials and Welding 2021. This is the CCS rule, not an IACS unified requirement: IACS UR W28 needs a free IACS login to download and was not checked. Your society's own rules govern.
This planning aid does not constitute an approval. The approval certificate issued by your classification society states the approved range. For plate ready to ship, contact us. Request a quote
Common questions
- Why do fillet welds need a multi-pass test?
- Table 3.1.4.5a lists fillet welds only in the multi-pass column. A single-pass test gives a range for butt and T joints and does not list fillet welds.
- Why does heat input change the result?
- Above 50 kJ/cm the rules cover fewer steels, cap the approved thickness at the tested thickness, and add an impact notch position. Above 200 kJ/cm they add one more.
- Why does the planner say to confirm some steels with the society?
- For steels of lower strength, clause 3.1.4.3 (2) gives the strength range but says nothing about toughness. If the steel to be welded is a tougher grade than the test steel, the rule does not answer, so the planner does not either.