Shipbuilding steel plate

AH36

Core stockMulti-class certified

This higher-strength class carries impact testing at 0°C. Higher yield strength allows thinner sections for the same load-bearing capacity, commonly specified for larger bulk carriers, tankers and container ships.

Mechanical properties

Grade class
Higher strength
Minimum yield ReH
355 MPa
Tensile strength Rm
490–630 MPa
Elongation A5
21%
Impact test temperature
0 °C

Impact energy in joules is not listed here because it varies with plate thickness and specimen orientation. The value that governs your order is the one on the mill test certificate, issued per heat.

Impact toughness for AH36 is verified by Charpy V-notch testing at 0°C, per IACS UR W11.

Definitions of ReH, TMCP and other terms: see the glossary

Chemical composition

Ladle analysis limits in weight per cent, as the WISCO mill publishes them for this grade to CCS. Als is acid-soluble aluminium.

CMnSiPSAlsNbV
≤ 0.180.90 – 1.60≤ 0.50≤ 0.035≤ 0.035≥ 0.0150.02 – 0.050.05 – 0.10

These are the mill's published limits for ladle samples. The actual values for your plate are on the mill test certificate, and a classification society can ask for tighter limits.

Stock & dimensions

Thickness
5–22 mm
Widths
1,800 / 2,000 mm
Lengths
8,000 / 10,000 mm

Mill rolling range

Sizes the WISCO mill rolls to order, beyond what is held in stock. Supplied to GB 712 and to the rules of BV, CCS, DNV, GL, LR, KR, NK and RINA, with dimensional tolerance to GB/T 709 and a lower thickness deviation of −0.30 mm. Send the requirement for availability and a lead time.

Thickness
2–19 mm
Widths
900–2,100 mm
Lengths
2,000–12,000 mm

Also rolled as coil

Original coil
2–19 mm × 900–2,100 mm
Skin-pass coil
2–12.7 mm × 900–2,100 mm

Coil sizes are the ranges in the mill's own product table. Confirm coil availability before you plan around it.

Thickness tolerance reference (EN 10029 / ASTM A6)

Currently in stock

ThicknessWidthLengthAvailability
8 mm1,800 mm10,000 mmEnquire
10 mm1,800 mm10,000 mmEnquire
12 mm1,800 mm10,000 mmEnquire
8 mm2,000 mm10,000 mmEnquire
10 mm2,000 mm10,000 mmEnquire
12 mm2,000 mm10,000 mmEnquire

Also supplied as bulb flat

AH36 is also held as bulb flat bar for hull framing.

View bulb flat availability

Low-residual-stress option available

AH36 is also available as low-residual-stress hot-rolled plate — lower residual stress, less warping after cutting and welding. Developed and validated with CSSC Guangzhou Shipyard International, and already in batch use on car-ferry and tanker thin-plate structures.

About low-residual-stress plate

Classification society approvals

Plate is produced at the WISCO mill, which holds works approval from the nine classification societies below. Plate is released with the mill test certificate for the relevant heat.

  • CCS AH36
  • ABS AH36
  • DNV AH36
  • GL AH36
  • BV AH36
  • LR AH36
  • RINA AH36
  • KR AH36
  • NK AH36

Bulb flat bar in this grade is produced at the Hubei Lijin mill and at Jufeng. Hubei Lijin holds works approvals from eight classification societies for bulb flat steel and sections; the certificates and the scope of each are on the certifications page. Bulb flat is released with the mill test certificate for the relevant heat. See the Lijin approval certificates

How to read a mill test certificate

Standards & cross-reference

This grade is also recognized under ASTM A131/A131M (the U.S. shipbuilding-steel specification) and GB/T 712 (the Chinese national shipbuilding-steel standard), both of which use the same AH36 designation as the IACS classification-society rules.

General structural-steel standards such as EN 10025 (Europe) and JIS G3106 (Japan) lack classification-society approval for ship hulls and cannot replace AH36 on a classed vessel. AH36 vs A36

Quick answers

What is the lead time for AH36 plate from ZCMetals?

AH36 is held in stock in Wuhan — ex-warehouse delivery in 3–7 days from order confirmation.

What certificate ships with AH36 plate?

A mill test certificate (MTC) to EN 10204 3.1, issued per heat, plus a classification society certificate copy for whichever of our nine approved societies your project requires. Independent third-party witnessed inspection (EN 10204 3.2) can be arranged on request.

What is the minimum order quantity for AH36?

From 1 tonne on sizes already held in stock — bundles are broken to order.

Welding & cutting

Cutting

Both oxy-fuel (flame) and plasma cutting are suitable for this thickness range; cut to your drawing or DXF file.

Welding & preheat

Higher-strength grades (AH32/AH36 series) have a higher carbon equivalent than normal-strength grades, so thicker sections or restrained joints may call for preheat and low-hydrogen consumables to avoid hydrogen cracking. Exact preheat temperature depends on thickness, carbon equivalent and joint restraint — confirm against your yard's WPS and the classification society's requirements rather than a fixed rule of thumb.

Related grades

Grade selection guide
AH32 vs AH36 steel plateAH36 vs DH36 steel plate

Tell us the grade, thickness and tonnage.

Send grade, thickness, dimensions and tonnage. You get availability, price and a lead time, normally within 24 hours.

Request a quick quote

Enquire about AH36Message on WhatsApp